Description
Can avoid the scratch, stain and fracture of Aluminum profile in the process of transportation.installation and useand reduce the loss of products.
No convex roll.
Custion width min. 1cm.
Suitable for various profile finish.
Easy to stick and tear.
ilm blowing process | 3 layer coextrusion |
Recommended thickness | 60mic, 800mic, 120mic, 130mic, 150mic; |
Recommended length | 200m,300m, 500m; |
Recommended width | 20mm – 1250mm; |
Colour | black and white, milky white, Transperent; |
Printing | up to 3 colour |
Core diameter | 76.2mm |
Product performance | lazer cutting, Stamping forming, Scratch proof, puncture resistant, Dust proof and antifouling; |
Recommended Peel Strength | smooth 300g/25mm, Matte 500g/25mm, powder coated 600g/25mm; |
Recommended glue amount | 17g/㎡, 45/㎡, 60/㎡; |
Tensile strength transverse | >20N |
Tensile strength longitudinal | >20N |
Elongation transverse | 500%-600% |
Elongation longitudinal | 500%-600% |
Storage conditions | Cool and dry place for one year |
Service conditions | Use below 70 ℃,Tear off the protective film within 60 days (except for special properties) |
Advantages | Anti convex roll, Easy to tear, easy to stick, no residual glue, firm printing; |